  • IMPC
    Leaching Behavior of Cu, Bi and Sb from Trof Furnace Doré Slag during Mineral Acid Leaching

    By P. Latostenmaa, T. Hailemariam, M. Lundström, P. Halli

    Doré process is unique way to treat precious metals in the copper electrorefining plant, since it uses anode slime as a raw material. In this pyrometallurgical process, also slag is produced together

    Jan 1, 2018

  • AUSIMM
    Leaching Behavior of Gold in Iodide Solutions

    By Qi P. H

    Gold dissolution can be achieved with a number of complexing ligands, all with varying degrees of stability. Processes based on the use of halogens have been known for many years. Beside providing t

    Jan 1, 1991

  • SME
    Leaching behavior of lithium from bauxite residue using acetic acid

    By Ning Wang, Tengfei Guo, Wanyan Li, Hanjie Wen, Hannian Gu, Zehai Li

    Red mud has been reported as a potential resource for lithium. To investigate the leaching behavior of lithium, a lithium-rich red mud was neutralized with hydrochloric or oxalic acid and then leached

  • SME
    Leaching Behavior of Lithium from Bauxite Residue Using Acetic Acid Mining, Metallurgy and Exploration

    By Ning Wang, Tengfei Guo, Wanyan Li, Hanjie Wen, Hannian Gu, Zehai Li

    Bauxite residue (red mud) is an alkaline waste derived from the industrial process for extraction of alumina from bauxite ore. Some bauxite residues contain considerable concentrations of critical met

  • SME
    Leaching Behavior of Lithium from Bauxite Residue Using Acetic Acid Mining, Metallurgy and Exploration (1c2dd284-40d8-467a-9f57-cf193eac1926)

    By Ning Wang, Tengfei Guo, Wanyan Li, Hanjie Wen, Hannian Gu, Zehai Li

    Bauxite residue (red mud) is an alkaline waste derived from the industrial process for extraction of alumina from bauxite ore. Some bauxite residues contain considerable concentrations of critical met

  • SME
    Leaching Behavior Of Palladium In Thiourea/Acid Solutions

    By K. N. Han, X. Xie

    The dissolution behavior of palladium powder in thiourea solutions was investigated. The variables studied were temperature, stirring speed and the concentrations of thiourea, acid and ferric ion. Pal

    Jan 1, 1997

  • CIM
    Leaching Behavior of the Roasted Nickel Calcine

    By D. Yu, T. A. Utigard, M. Barati

    "Sulfation roasting of nickel concentrate to generate water-soluble metal sulfates was investigated as an alternative process to smelting for the recovery of valuable metals. The kinetics of dissoluti

    Jan 1, 2012

  • CIM
    Leaching Behaviour and Metal Fixation Within Cemented Paste Backfill Materials

    By E. Fried

    Cemented paste backfill (CPB) is an innovative tailings management method that consists in returning considerable amounts of mine tailings into the underground mine openings. The filled stopes thus pa

    May 1, 2007

  • IMPC
    Leaching Behaviour And Particle Interactions In Uranium Laterite Dispersions: Effect Of Ore Mineralogy And Temperature

    Due to complex mineralogical and chemical interactions of the value and gangue mineral phases present in uranium-containing lateritic ores, deleterious pulp gelation which impacts on value metal recov

    Sep 1, 2012

  • CIM
    Leaching Behaviour of a Colombian Nickel Laterite in Aqueous Alkaline Glycine Solutions

    By G. T. Lapidus, A. Garcés, O. J. Restrepo

    "Colombian nickel laterites have historically been processed by pyrometallurgy. However, due to the depletion in ore grades, alternative processes are required. Hydrometallurgical processes, such as p

    Jan 1, 2017

  • CIM
    Leaching Characteristics of a Low-Grade Nickel-Bearing Ore Upgraded on the Falcon Concentrator

    By M. B. Shongwe, R. K. K. Mbaya, C. K. Thubakgale, P. Mendonidis

    "A low-grade nickel-bearing ore was pre-concentrated on a SB40 laboratory model Falcon Concentrator. Three size fractions, -212+125, -125+75 and -75 µm were tested with the intent to upgrade the nicke

    Jan 1, 2017

  • AUSIMM
    Leaching Characteristics of Australian Uranium Ores

    The leaching characteristics of a number of Australian uranium ores were determined under acid and alkaline conditions. Ores from the Ranger, Nabarlek and Koongarra deposits in the Northern Territory

    Jan 1, 1979

  • SAIMM
    Leaching characteristics of cerium and yttrium from non-magnetic coal fly ash after silicate digestion using acetic acid

    By H. Manurung, I. M. Bendiayasa, W. Astuti, and H. T. B. M. Petrus, F Anggara, K. C. Wanta

    The leaching kinetics of cerium (Ce) and yttrium (Y) in sodium-hydroxide-digested non-magnetic coal fly ash using acetic acid were investigated. The variables analysed were pH, solid-to-liquid ratio (

    Nov 6, 2024

  • SME
    Leaching Characteristics Of Copper Refractory Ore In Sulfate Media

    Refractory copper ores (CROs) in central Africa contain copper minerals that are locked up in a micacious solid matrix or associated with carbonate, sulfide and phosphate minerals. Several researchers

    Jan 1, 2011

  • SME
    Leaching Characteristics Of Copper Refractory Ore In Sulfate Media (72fefa33-b60e-41f5-b286-1b56b05d7e4d)

    Refractory copper ores (CROs) in central Africa contain copper minerals that are locked up in a micacious solid matrix or associated with carbonate, sulfide and phosphate minerals. Several researchers

    Nov 1, 2011

  • IOM3
    Leaching characteristics of heavy metals from three historical Pb-Zn mine tailings heaps in the United Kingdom

    By G. Merrington, B. J. Alloway

    Tailings from three historical mining areas in the UK were leached in columns under a simulated weathering programme which was chosen to represent periods of 1 and 2 years at 3 different ambient tempe

    Jan 8, 1993

  • CIM
    Leaching Characteristics of Nickeliferous Pyrrhotite Tailings from the Sudbury, Ontario Area

    By Elizabeth Edwards, Radhakrishnan Mahadevan, Vladimiros G. Papangelakis, Srinath Garg, Kurtis Judd

    Mineralogical characterization of the tailings showed the deportment of Ni to be similar in the Vale and Glencore tailings, with 60% of the total Ni locked in pyrrhotite, and the balance 40% associate

    Jan 1, 2017

  • IMPC
    Leaching Complex Gold Ores

    Calaverite is a gold telluride found in the Kalgoorlie region, Fiji, Cripple Creek Colorado and numerous other locations. It is known that a high pH is necessary for calaverite cyanidation, with the l

    Jan 1, 2014

  • CIM
    Leaching Concentrates without Leaching Iron

    By M. Maccagni, J. Nielsen

    "Engitec developed the EZINEX® Technology some years ago to recover zinc from oxidized secondary sources. This process works at neutral pH and can take into solution any kind of metal, but iron is re

    Jan 1, 2016

  • AIME
    Leaching Copper from Worked-Out Areas of the Ray Mines, Arizona

    By Robert W. Thomas

    LEACHING of mined-out areas at the Arizona property of the Ray Mines Division, Kennecott Copper Corp., was started on Jan. 20, 1.937, and by July 1, 1938, 10,000,000 lb. of copper had been produced by

    Jan 1, 1938