Search Documents
Search Again
Search Again
Refine Search
Refine Search
-
Rigs From Iron Containing Dusts & Sludges
By Christopher M. Moore
DK Recycling und Rohelsen GmbH converts 380 000 annual tonnes of iron containing waste materials Into pig Iron. Zinc Is the main reason that these materials are classified as waste. The materials are
Jan 1, 1995
-
Effect Of Additives On The Viscosity Of Molten Nickel Base Alloys
By Yuzura Sato
Viscosity has been measured for various molten binary alloys of nickel with iron, cobalt and chromium in order to clarify the behavior of viscous flow of molten nickel alloys. The entire concentration
Jan 1, 2003
-
Study of the Diffusion of Cu(II) as an Oxidant Through Simulated Particle Pores in a Novel Model Apparatus
By B. Manana
In heap leaching, the oxidative dissolution of value minerals encapsulated deep within large particles cannot be fully understood on the basis of the bulk solution conditions relative to variable solu
-
Integrated Pyrorefining of Lead at Teck’s Trail Operations
By G. Richards
The Trail smelter of Teck Metals Ltd. produces about 90,000 tonnes of lead per year through two stages of refining following KIVCETTM smelting. Bullion from the KIVCET furnace is first treated in a py
-
Refractory Corrosion by Ferrite Slag at Elevated Temperatures
By K. Yarnaguchi
In the Mitsubishi Continuous Copper Converting Furnace, calcium femte slag is used. Due to its extremely high basicity, the improvement of corrosion resistance of the refractory lining is in need. In
Jan 1, 1994
-
Integrated Recycling Of Non-Ferrous Metals At Boliden Ltd. Rönnskär Smelter
By Theo Lehner
The Rönnskär smelter has wide experience in the field of recycling of non-ferrous metals. Today, smelting and refining from primary and secondary raw materials are integrated in a complex flow sheet.
Jan 1, 1998
-
Improved Converter Control
By J. -P. Nepper
It has been possible to largely contain converter aisle emissions of SO2 and fumes in the case of batch-wise operated Peirce Smith converters during normal blowing periods with the help of suitably de
Jan 1, 1992
-
Sirosmelt Technology For Solving The Lead And Zinc Industry Waste Problem
By K. R. Robilliard
An outline is given of the problems facing tlile lead and zinc industry from the viewpoint of the range of residues currently produced from electrolytic zinc, blast furnace and other processes. Smel
Jan 1, 1992
-
The Contribution Of Pyrometallurgy To Sustainable Development (Keynote)
By W. K. Rankin
Achieving continued economic growth with social equity within the natural limits of the Earth's eco-systems is the major issue facing the world today. The material and energy needs of the world c
Jan 1, 2003
-
Computational Modelling Of Freeze Layers in Smelting Processes
By Mark Cross, Andrew P. Campbell, Koulis A. Pericleous
"Computational Fluid Dynamics (CFD) modelling is being used to simulate the freeze layers formed within direct smelting processes. There has been some concern whether water-cooled elements can withsta
Jan 1, 2001
-
Recovery Of Uranium Using Continuous Countercurrent Ion Exchange,(CCIX)
By Joseph C. Milbourne
Tetra Technologies CCIX? (continuous countercurrent ion exchange) system has been involved in a wide range of uranium concentration, separation and purification applications over the past 40 years. Ur
Jan 1, 1995
-
Upcoming Zinc Mine Projects: The Key for Success is Zincex Solvent Extraction
By A. Mejias, M. A. Garcia, G. Diaz
During 1997 and 1998 two successful zinc feasibility studies, Skorpion and Sanyati, were carried out by Tecnicas Reunidas based on the modified ZINCEX® technology. The technical viability of each proj
Jan 1, 2000
-
Equipment Selection for Chloride Circuits
By G. R. Waters
NMR360 is developing a suite of chloride-based metals extraction processes, with the first commercial operation scheduled for commissioning late in 2018. It is critical, therefore, that with the intro
-
Measurement of Liberation of Finely Ground Iron Ores
By William A. Hockings
Methods for the measurement of liberation of finely ground iron ores are described. The general method consists of separating a sample of the ground ore into a number of size fractions, followed by me
Jan 1, 1981
-
Solubility of Germanium Dioxide in Commonly Used Acids—Effect of Acid Strength, Temperature, and Water Activity
By T. Feldmann
Despite the ubiquity of applications for germanium, there is a lack of practically useful solubility data in acidic solutions. Previous studies were done at ambient temperature and only for commonly u
-
Installation Of Arsenic Removal In The Hematite Process (c1cda2c1-a9fd-43db-8e83-1dd87fe69bec)
By H. Masuda
The lijima Zinc Refinery started operation in 1972, and has today an annual capacity of 200, 000+-Zn. The hematite process was employed for the first time and the ideal of waste-free refinery has been
Jan 1, 2003
-
Prediction of Austenite Decomposition During Cooling of Low and Medium-Carbon Low-Alloy Steels
By E. Anelli
Based on experimental continuous cooling transformation (CCT) diagrams, an artificial neural network has been trained to predict the amount of microsturctural constituents and hardness resulting from
Jan 1, 2003
-
Kinetics of Oxidation of Pyrrhotite
By Anastasia Alksnis
Pyrrhotite is an iron deficient, low nickel content sulfide mineral that is commonly associated with pentlandite, a nickel-rich sulfide; and are both main components of the nickel ore mined in Sudbury
-
Forging Process Design in a Concurrent Engineering Environment
By Bin Du
In recent years, concurrent product design and process is gaining popularity and will become a norm of the industry of the future. Forging has been a critical manufacturing process for production of c
Jan 1, 1992
-
Ultra-High Purification of Transition Metals by Anion Exchange Applying Various Oxidation States
By Kouji Mimura, Tamas Kekesi, Yongfu Zhu, Masahito Uchikoshi, Minoru Isshiki
"The formation and anion exchange sorption of chloro complex ions can offer a great potential to be utilized for the separation and purification of metals in aqueous solutions. Available stability dat
Jan 1, 2000