Search Documents
Search Again
Search Again
Refine Search
Refine Search
-
Lead Recycling from Automotive Batteries: an Hydrometallurgical Case StudyBy Ramon V. V de Araújo, Roberto B. E Trindade, Pablo R. Fica-Piras
"Lead has been reported to affect blood vessels and kidneys. It also produces adverse effects in the mental and physical development of children and nervous system of adults. It is also considered as
Jan 1, 2003
-
Kinetic Features In Collective Flotation Of Sulphide MineralsBy Antoineta Boteva
A significant part of the currently production of the non-ferrous and precious metals is from sulfide ores. Character feature of sulfide ores is the presence in them always pyrite and wide range of di
Sep 1, 2012
-
Breakage Characteristics Of Pyrophyllite In A Laboratory Ball MillBy Hoon Lee
Laboratory tests were conducted to evaluate the breakage characteristics of pyrophyllite in a laboratory ball mill. In grinding tests, the breakage characteristics were analyzed using the mathematical
Sep 1, 2012
-
Refractory Gold Treatment-State Of The Art And Future ChallengesBy Robert Dunne
A review of the current ?state of the art? of refractory gold treatment will be provided. This will include a global perspective of the refractory processes that are being practiced, where they are an
Sep 1, 2012
-
Vale - Transforming Natural Resources Into Wealth & Sustainable DevelopmentAs a leading global company in the mining sector, we are committed to sustainable development. To this end, we invest in the responsible, integrated management of economic, environmental and social is
Sep 1, 2012
-
Advanced Modeling Techniques In Mineral Processing And Their Influence On Our IndustryBy John A. Herbst
Professor A.M. Gaudin and his students at MIT were dedicated to understanding the fundamentals of mineral processing and as a consequence were constantly searching for better quantatative descriptions
Sep 1, 2012
-
Analysis Of Ball Mill Grinding Operation For Scale-Up And DesignBy V. K. Gupta
Selection of mill size for reducing a feed material of a given size to the desired product size is generally based on the specific energy estimate obtained from Bond test. Over the last thirty years o
Sep 1, 2012
-
New Dimensions In Advanced Process Control Of Mineral Processing PlantsBy Alain Broussaud
The lecture is about the growing role and the evolution of advanced process control (APC) in the mining and mineral processing industry, taking into account major trends in Information Technology. It
Sep 1, 2012
-
Beneficiation Of Iron Ore Slimes From Bellary-Hospet, IndiaBy B. Suresh
Iron ore in Bellary-Hospet region is friable in nature and generates a significant amount of micro-fines (-150 µm) during mechanized mining, handling and processing. Present beneficiation practice gen
Sep 1, 2012
-
Flotation of selected copper sulfide minerals in saline watersBy Kevin Davey, Liza Forbes, Leanne Smith
Given the global scarcity and value of potable water, interest in the use of water of lower quality in mineral processing has grown significantly in recent years. Previous laboratory batch flotation t
Jan 1, 2014
-
MillStar and FloatStar advanced process control system at a silver (Ag) concentratorBy Sydney Mantsho, Toni Streczynski, Manuel Gonzalez
"In 2013, the commissioning of the MillStar Stabilisation and FloatStar Stabilisation and Optimisation controllers were completed at the Cerro Bayo Silver (Ag) mine in Patagonia, Chile. The MillStar c
Jan 1, 2014
-
Sustainable Development: Challenges Faced In Mineral ProcessingBy Hemant Nerurkar
The destination of human development journey is envisioned as human well being. Human well-being is the extent to which individual share the ability and the opportunity to live the kinds of lives they
Sep 1, 2012
-
Effects of Picobubbles by Hydrodynamic Cavitation on Coarse Phosphate Froth FlotationBy M. M. Fan
In Florida?s phosphate industrial practice, the most favorable upper size limit of froth flotation is 1.18 mm which corresponds to particle weight of about 2.8 mg. Conventional froth flotation is not
Jan 1, 2014
-
Technology for gold recovery from poor argillaceous oxidized ores by a combined methodBy Arkady Senchenko, Andrey Vasiliev, Alexander Aksenov, Metodi Zlatev
"This paper considers the issue of treating argillaceous oxidized ores with low gold grade (around 1.0 g/t). These ores according to their gold recovery level can be treated by heap leaching and agita
Jan 1, 2014
-
Holistic Approach On ?Sustainable Growth? Of Mineral Processing IndustriesBy T. C. Rao
This presentation identifies how mineral (coal included) processing profession should look at the challenges (threats) being faced by mineral industry. Presently, the focus is more on supply and deman
Sep 1, 2012
-
The investigation of operating parameters in a vertical stirred millBy Garren Edwards, van der Westhuizen. Andre
"Due to the depletion of easily treated coarser ores, more mineralogically complex ores with smaller valuable mineral grain sizes are treated, the means to liberate these minerals lies in grinding fin
Jan 1, 2014
-
Thickening and deposition trials: Laboratory through to industrial scale - Minera EsperanzaBy F. Bello, J. Engels
"During 2012 and 2013, Minera Esperanza conducted a series of thickening and deposition trials to identify design and operational parameters associated with increased thickening of its tailings. These
Jan 1, 2014
-
Laboratory Tests on the Production of High Quality Zeolite (9579e8a5-2c38-4a64-bcca-678557289c30)By Güven Önal, Gülay Bulut, Mustafa Özer, Yunus Emre Benkli, Olgaç Kangal, Mustafa Tarkan
There are various types of natural zeolite deposits in Turkey. Naturally occurring zeolites are excluded from many important commercial applications where uniformity and purity are essential. In this
Jan 1, 2003
-
Impact of mill size on low-energy surface damageBy Nirmal S. Weerasekara, Malcolm S. Powell, Mohsen Yahyaei
"An understanding of the fundamentals of different breakage mechanisms is critical for successfully modelling comminution processes. Due to the high frequency of low energy collisions in the grinding
Jan 1, 2014
-
Increasing Final Concentrate Grade of the Sarcheshmeh Copper Complex Flotation Circuit by Flowsheet ModificationBy S. Banisi, E. Arghavani, M. Pourkani, M. J. Rajabi, Gh. A. Mohamadian, H. Bidshahri, Gh. A. Parsapour
The Sarcheshmeh copper complex flotation circuit of plant No.1 consists of two identical north and south sections where each includes four rougher (each bank consists of 14 cells), two cleaners (each