Leaching Sulfur from Pressure Acid Leaching Residue of Zinc Concentrate: Parameter Optimization Using Response Surface MethodologyBy Peng Peng, Ouo Cheng, Guodong Lai, Lijuan Chu, Zebiao Zhang
"The pressure acid leaching residue of zinc concentrate contains a large quantity of sulfur. The present study attempts to leach sulfur using a mixture of ammonium sulfide and water solution at 25°C.
Jan 1, 2012
-
EDXRF Analysis Of Alloys And Corrosion Products Of Metallic Pre-Hispanic Pieces Of The Museum Of Ethnology And Archaeology Of The University Of Sao PauloBy A. C. Neiva
An energy-dispersive x-ray fluorescence spectrometer was assembled with the aim of analysing alloys and corrosion products of artistic, ethnological and archaeological pieces. The spectrometer is semi
Jan 1, 2006
-
Spouted Bed Electrowinning of Zinc from Chloride ElectrolytesBy C. Allen, A. Roy, J. W. Evans
A spouted bed electrode (SBE) has been used, in laboratory experiments, to electrowin zinc from zinc chloride electrolytes with the objective of determining the suitability of this electrode for comme
Jan 1, 2000
-
Electrochemical destruction of free cyanide on a cobalt oxide doped electrodeBy E. Fockedey
he destruction of free cyanide on a Co3O4 doped carbon felt was studied. The experiments were done with an eiectrochemical filter press cell on dilute alkaline solutions containing 250 mg/l NaCN. No
Jan 1, 1998
-
Viscosities Of FeNO-MgO-SiO2 And FeNO-MgO-CaO-SiO2 Slags (2ac3a2ff-8b6a-455b-99e0-64c885cdd714)By Dai Xi
In the present work, the viscosities of molten FenO-MgO-SiO2 and FenO-MgO-CaO-SiO2 semi-synthetic slags for nickel flash smelting were measured in the temperature range from 1473 to 1723K by a rotatio
Jan 1, 2003
-
Detection of Creep Damage in a Nickel Base Super-Alloy by Nondestructive MeansBy Hector Carreon
Due to elevated temperatures, excessive stresses and severed corrosion conditions, turbine engine components are subject to creep processes that limit the components life such as a turbine bucket. The
Jan 1, 2010
-
Rare-Earth Elements Recovery from Nd-Fe-B Hard Magnets by Hydrometallurgical ProcessesBy Haydar Güneş
In this study, a hydrometallurgical process was evaluated for the recovery of Nd from a Nd-Fe-B magnet. Each leaching test was performed at the solid (weight) to liquid (volume) ratio of 1:50 and was
-
Characterization and Leaching Proposal of Ag(I) from a Zn Concentrate in an S2O3(2-)-O2 MediumBy Juárez T. Julio Cesar, Mendez R. Eliecer, Reyes P. Martín, Flores G. Mizraim Uriel, Teja R. Aislinn Michelle, Hernández C. Leticia, Reyes D. Iván Alejandro
The present study shows the characterization of a zinc concentrate collected at Hidalgo, Mexico, in order to identify its mineralogical species and to propose a leaching methodology for silver recover
Mar 1, 2017
-
Common Granulation System Problems With A Focus On Non-Ferrous ApplicationsBy Art Cooper
Granulation systems are customarily viewed as problem areas in metallurgical operations. The inherent risk of explosion when combining a high temperature melt with water creates a safety hazard. Separ
Jan 1, 2006
-
Preliminary Research on Preparation Al-Si-Ti Alloy With Aluminum Ash as Electrolysis MaterialsBy Qingsheng Liu
A new method of recycling aluminum dross for preparation Al-Si-Ti alloy was studied in this paper. This was carried out in two processes. first the aluminum doss was pretreated by leaching and calcini
Jan 1, 2010
-
Treatment of Residues During Aluminum RecyclingBy Ramona Prillhofer
Salt slag is a waste product produced by the recycling of aluminum. In most European countries (e.g. Austria, Germany) the landfill disposal of this waste is forbidden because the slag contains solubl
Jan 1, 2009
-
Remediation of Chicken Processing Wastewater using Electrochemically Produced Layered Double HydroxidesBy Jewel A. G. Gomes
Green rust (GR) are layered Fe(II)-Fe(III) double hydroxides, having a pyroaurite-type structure consisting of positively charged hydroxide layers and hydrated ions in interlayers. This special featur
Jan 1, 2010
-
Advances In Understanding Of Phenomena In The Blast Furnace HearthBy Pinakin C. Chaubal
An industry ? university consortium was set up to develop advanced tools necessary to understanding of the various phenomena occurring in the hearth of the modern iron making blast furnace. The major
Jan 1, 2006
-
High Oxygen Shrouded Injection At Falconbridge: Five Years Of OperationBy Joël P. T. Kapusta
Although Peirce-Smith converting remains the workhorse in matte converting, the copper and nickel industries are still confronted with production hindrances such as tuyere blockage, excessive refracto
Jan 1, 2005
-
Investigation of Optimum Cementation Conditions of Ruthenium with Experimental DesignBy B. Zeytuncu, O. Yucel, O. H. Celik, M. H. Morcali
"The Taguchi method was used as the experimental design to determine the optimum conditions of cementation behavior of the ruthenium chloride solution. Cementation was carried out using metallic zinc
Jan 1, 2013
-
Sustainability Study in Selective Laser Sintering ? An Energy PerspectiveBy Rameshwar Sreenivasan
This paper presents a sustainability analysis of Selective Laser Sintering (SLS) from an energy standpoint. Data of electrical power consumed by the system over an entire build were acquired using a L
Jan 1, 2010
-
A Recovery Technology of Ag from Composite Ag-Cu Electronic WastesBy Jinhui Li
Silver is a very important metal used in a wide range of applications. It is necessary to recovery of Ag from electronic wastes for increasing of Ag price and circumstance protection. For separating a
Jan 1, 2009
-
Reduction Behavior of Ternary Calcium Ferrites for CaO-Fe2O3-MgO SystemBy Chengyi Ding, Xuewei Lv, Senwei Xuan, Chenguang Bai, Kai Tang, Gang Li
Sinter is an important iron-bearing material charged into blast furnace. Calcium ferrite (CF) is one of the most significant liquid phases in fluxed sinter. The isothermal reduction kinetics of CF and
Mar 1, 2018
-
Remediation Of Acid Mine Drainage At The Friendship Hill National Historic Site With A Pulsed Limestone Bed ProcessBy Philip L. Sibrell
A new process utilizing pulsed fluidized limestone beds was tested for the remediation of acid mine drainage at the Friendship Hill National Historic Site, in southwestern Pennsylvania. A 230 liter-pe
Jan 1, 2003
-
A New Process for the Decontamination of Industrial Effluent Containing Cadmium CationsBy I. Gaballah
Cadmium is toxic to plant, animals and humans. The council directive of the European Communities No 8315 13lEEC has fixed an upper limit of 200 ppb for the release of cadmium in industrial effluents.
Jan 1, 1994