Abstract
SOME years ago, the writer described heat checks or thermal. cracks that occur in die-casting dies.1 The life of dies was considered in relation to the casting temperature, the material used for the die, and the heat to be absorbed by the die per unit volume of casting made. The mech-anism of the action that results in thermal failure of dies was described. In the present paper the writer proposes to describe some additional observations in regard to heat checking, make one or two suggestions as to the method or methods for further attack of the problem, and give the results obtained on some work carried out along these lines.
Citation
APA:
(1934) Steels for Die-casting Dies (2f71af5f-98e3-4b02-beca-7f0d2ee74f1c)MLA: Steels for Die-casting Dies (2f71af5f-98e3-4b02-beca-7f0d2ee74f1c). The American Institute of Mining, Metallurgical, and Petroleum Engineers, 1934.