Separation Of Enargite From Cu-Concentrate

International Mineral Processing Congress
K. Haga
Organization:
International Mineral Processing Congress
Pages:
11
File Size:
439 KB
Publication Date:
Sep 1, 2012

Abstract

In this study, flotation tests were performed to investigate behavior of enargite and chalcopyrite ores from different sources synthetically mixed for separation of enargite. Flotation parameters including; pH, reagents concentration and type and flotation time were controlled to obtain an enargite concentrate with high As and chalcopyrite concentrate and final tailings with As content below 0.5 mass%. The copper ore bearing enargite mineral contained 5.87 mass% As and 16.50 mass% Cu while the chalcopyrite bearing ore contained 0.32 mass% As and 21.63 mass% Cu. The two ore samples were mixed at 7:3 (enargite: chalcopyrite) by weight ratio to prepare a mixed ore sample with arsenic content at 3.16 mass% and 18.25 mass% Cu for the flotation study. For enargite single ore flotation, the 38?75 µm size fraction showed that over 98% enargite was selectively recovered within 5 min at slurry pH of 4.0 and arsenic content in the final tailings was reduced to 0.22 mass%. In mix ore (enargite+chalcopyrite) flotation, 97% of enargite was first removed at pH 4 followed by chalcopyrite flotation at pH 8, and over 95% recovery was achieved in 15 min flotation time. Arsenic content in the final tailings was reduced to 0.1 mass%.
Citation

APA: K. Haga  (2012)  Separation Of Enargite From Cu-Concentrate

MLA: K. Haga Separation Of Enargite From Cu-Concentrate. International Mineral Processing Congress, 2012.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account