Abstract

Solid state reduction of roast movat chromite ore with carbon was carried out as a function of C/FeO ratio and temperature in the range 800°C to 900°C by thermogravimetry analysis (TGA). A two stage mechanism, (1) the reduction of FeO present in Roast Movat with carbon monoxide; and (2) the regeneration of CO by the oxidation of carbon with CO2 was proposed. The rate controlling step is the carbon oxidation reaction. A kinetic equation, that of random nucleation, was proposed. The activation energy for the reduction was determined to be 55800 J/mole and is compared to those activation energies determined for other chromite ores.
Citation

APA: R. G. Reddy  (1998)  Reduction Of Roast Movat Chromite Ore With Carbon (2060f1ae-dad6-4029-850c-5f4b4224af19)

MLA: R. G. Reddy Reduction Of Roast Movat Chromite Ore With Carbon (2060f1ae-dad6-4029-850c-5f4b4224af19). Society for Mining, Metallurgy & Exploration, 1998.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account