Recovery of Copper. Cobalt and Nickel from Divrigi Sulfide Concentrates

The Minerals, Metals and Materials Society
E. Açma
Organization:
The Minerals, Metals and Materials Society
Pages:
17
File Size:
300 KB
Publication Date:
Jan 1, 1993

Abstract

Sivas-Divrigi flotation plant has a capacity of 90,000 tpy. Beneficiation of the tailings of iron ore magnetic separator seems to be attractive, because of its Cu, Co, and Ni contents. In the experimental work, sulfidic flotation concentrate is produced from these tailings. A roasting-leaching-H2S precipitation procedure is used to treat this concentrate, containing 0.55% Cu, 0.51% Co, 0.74% Ni, and 0.027% Zn. Sulfatizing roasting is carried out in a rotary furnace at 690°C. Roasted product is leached with 10 gpl HzSOl at 70°C and 30% pulp density. For the precipitation of desired metal, H2S is bubbled through the concentrated solution of repeated leaching, under controlled temperature and pH. Final metal recoveries of 91% Cu, 91% Co, and 50% Ni, and 92% Zn are attained. Roasting gases with their 13% SO2 content are suitable for H2SO4 production and the leach residues can be integrated with the iron ore processing plant as they contain 57.4% Fe and very low non-ferrous metals.
Citation

APA: E. Açma  (1993)  Recovery of Copper. Cobalt and Nickel from Divrigi Sulfide Concentrates

MLA: E. Açma Recovery of Copper. Cobalt and Nickel from Divrigi Sulfide Concentrates. The Minerals, Metals and Materials Society, 1993.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account