Preparing Strontium Carbonate with Celestite Concentrate by Agglomeration-reduction Roasting Process

International Mineral Processing Congress
G. H. Li
Organization:
International Mineral Processing Congress
Pages:
7
File Size:
347 KB
Publication Date:
Jan 1, 2014

Abstract

Preparation strontium carbonate with celestite concentrate by flotation is studied by agglomeration-reduction roasting process. It is shown that, the drop strength of green pellet is greater than 4 times?(0.5m) -1 under the balling conditions of moisture of 9% and time of 18~20min. Lignin xanthate obviously improves the ballability of the celestite concentrate due to the increase of surface hydrophilicity, therefore, the balling rate is increased, as well as green ball strength. The drop strength of 7 times?(0.5m) -1 can be obtained when the lignin xanthate dosage is 0.5%~1%. Reduction roasting with anthracite shows that the SrSO4 conversion is 82%~83% for celestite concentrate pellet, under the optimal conditions of roasting temperature of 1100~1150? and time of 30min, and it is 10% higher than conversion of celestite lump under the same conditions. The strontium carbonate are prepared after roasted pellets are leached, purified and carbonated, and the SrCO3 content is higher than 97% , while the content of CaCO3 is less than 0.3%.
Citation

APA: G. H. Li  (2014)  Preparing Strontium Carbonate with Celestite Concentrate by Agglomeration-reduction Roasting Process

MLA: G. H. Li Preparing Strontium Carbonate with Celestite Concentrate by Agglomeration-reduction Roasting Process. International Mineral Processing Congress, 2014.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account