Preparation Of Spherical Ultrafine Cobalt Powder By Polyol Reducing

The Minerals, Metals and Materials Society
Sheng-hai Yang
Organization:
The Minerals, Metals and Materials Society
Pages:
6
File Size:
2247 KB
Publication Date:
Jan 1, 2006

Abstract

The ultrafine, monodispersed, spherical cobalt powder has been fabricated by reducing cobalt hydroxide with glycol. It were investigated that the effect of NaOH concentration on the reaction rate and the effects of the concentration of cobalt hydroxide and surfactant on the morphology and particle size. The particles were characterized by the X-ray diffraction(XRD), scanning electron microscope(SEM), laser diffraction particle size analyzer and BET specific surface analyzer respectively. The XRD shows that the cobalt powders exist mostly in face centered cubic (fcc) structure, a little in simple hexagonal. The cobalt powders prepared at Co(OH)2150g/L, NaOH 40 g/L and surfactant 30g/L, its average particle size, specific surface area and cobalt content, were 0.88µm, 2.705m2/g. and more than 99.5% respectively.
Citation

APA: Sheng-hai Yang  (2006)  Preparation Of Spherical Ultrafine Cobalt Powder By Polyol Reducing

MLA: Sheng-hai Yang Preparation Of Spherical Ultrafine Cobalt Powder By Polyol Reducing. The Minerals, Metals and Materials Society, 2006.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account