Preparation of Iron Oxide Red by Acid Leaching Tailings

- Organization:
- International Mineral Processing Congress
- Pages:
- 5
- File Size:
- 298 KB
- Publication Date:
- Jan 1, 2014
Abstract
The utilization of acid leaching tailings was studied. It is obvious that the Fe in acid leaching tailings can be leached into solutions as Fe2+. In this paper, the influence of conditions, including the concentration of ferrous sulfate, pH, temperature and velocity of air flow was investigated. The optimum conditions for preparing seed crystal are as follows: the concentration of ferrous sulfate is 20 g/L; pH is 9.5~10; reaction temperature is 10~20?; velocity of air flow is 0.4m3/h. The optimum conditions for preparing iron oxide red are as follows: the concentration of ferrous sulfate is 5 g/L; reaction temperature is 80~85?; velocity of air flow is 0.13m3/h. At last, the product of iron oxide red could be prepared by ammonia method.
Citation
APA:
(2014) Preparation of Iron Oxide Red by Acid Leaching TailingsMLA: Preparation of Iron Oxide Red by Acid Leaching Tailings. International Mineral Processing Congress, 2014.