Pellet Feed Production Via The Concentration Of Flotation Tailings

Society for Mining, Metallurgy & Exploration
M. G. Vieira
Organization:
Society for Mining, Metallurgy & Exploration
Pages:
5
File Size:
2359 KB
Publication Date:
Jan 1, 2010

Abstract

This investigation addressed the possibility of producing pellet feed at a silica content of = 1.0% using a representative sample of Samarco´s mechanical flotation tailings. This sample contained 11.0% Fe and presented an F80 = 116 µm and a d50 = 63 µm. The higher silica content was verified in the coarser fractions and the higher iron content in the fraction -37 µm. Specular hematite is the most abundant mineralogical phase in the fraction -37 µm. The technological tests used one of four methods: magnetic concentration using a wet high-intensity magnetic separator, magnetic concentration using a SLon high-gradient magnetic separator, reverse flotation or direct flotation. The methods using the magnetic concentrator SLon, reverse flotation and direct flotation did not present results meeting the target of the study: iron content in the concentrate (rougher stage) greater than 34% or iron recovery greater than 80%. Cleaner stages were not achievable with the resulting concentrates. In contrast, the most successful method consisted of using wet high-intensity magnetic separators (WHIMS) as a rougher stage and reverse flotation as a cleaner stage. Using this route, it was possible to produce a pellet feed with a silica grade of 1.0% and high specular hematite content.
Citation

APA: M. G. Vieira  (2010)  Pellet Feed Production Via The Concentration Of Flotation Tailings

MLA: M. G. Vieira Pellet Feed Production Via The Concentration Of Flotation Tailings. Society for Mining, Metallurgy & Exploration, 2010.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account