Manufacturing of Incoloy800 Superalloy Strands in Continuous Casting Process with Electromagnetic Stirring
- Organization:
- Canadian Institute of Mining, Metallurgy and Petroleum
- Pages:
- 6
- File Size:
- 4328 KB
- Publication Date:
- Jan 1, 2014
Abstract
In this paper, the rectangular strands of Incoloy 800 superalloy were fabricated with a pilot vertical continuous caster in Northeastern University, China. In the processing, an electromagnetic stirring (EMS) is applied on the secondary cooling zone to control the solidifying structure and segregation of elements in the strands. The solidification structure of Incoloy 800 superalloy strands were investigated at different electric parameters and casting parameters. The research results show that the EMS can effectively restrain the dendrite growth and increase the ratio of equiaxed grains in Incoloy 800 superalloy strands as applied a suitable electric parameters and cooling condition in the process of continuous casting. The evolution of dendrite crystallization in Incoloy 800 alloy strands from the surface to its center during the solidifying process was investigated with and without EMS.
Citation
APA: (2014) Manufacturing of Incoloy800 Superalloy Strands in Continuous Casting Process with Electromagnetic Stirring
MLA: Manufacturing of Incoloy800 Superalloy Strands in Continuous Casting Process with Electromagnetic Stirring. Canadian Institute of Mining, Metallurgy and Petroleum, 2014.