Evaluation Of Lead-Zinc Flotation Tailings

- Organization:
- The Minerals, Metals and Materials Society
- Pages:
- 9
- File Size:
- 133 KB
- Publication Date:
- Jan 1, 2006
Abstract
Alada (Kayseri-Turkey) lead-zinc sulfide-oxide ores contain 10.17% Pb, 10.98 %Zn, 164 g/t Cd and 57 g/t Ag. During the laboratory scale flotation tests of these ores, it was found that almost all zinc was remained in the tailings that contain 12.31% Zn, 1.35%Pb, 198.3 g/t Cd, and 22.3%Fe. Three different methods were studied such as basic (NaOH) leaching, roasting+acidic (H2SO4) leaching and direct acidic (H2SO4) leaching for recovering metals that these tailings contain. In the direct acidic leaching, which gave the best results, dissolution efficiencies of 91.5% zinc, 78.2% cadmium, and 14.3% iron were reached at the optimum leaching conditions while Pb remained in the leach residues and the acid consumption was 422.3 kg/ton of tailings.
Citation
APA:
(2006) Evaluation Of Lead-Zinc Flotation TailingsMLA: Evaluation Of Lead-Zinc Flotation Tailings. The Minerals, Metals and Materials Society, 2006.