Effect Of Oxygen Enrichment On The Teniente Converter Productivity At The Ilo Smelter, Perú (67cdbd7e-3ac1-487c-b272-f30642fb3d30)

- Organization:
- The Minerals, Metals and Materials Society
- Pages:
- 8
- File Size:
- 308 KB
- Publication Date:
- Jan 1, 2003
Abstract
Low metal prices and environmental restrictions are always a challenge for copper smelters operation and its productivity. Thus, in order to reduce production costs and control gas emissions, improvements of the Teniente Converter (CT) operation were made at 110 Smelter Plant of Southern Peru Copper Co" 110, Peru, and the main objective was to increase its capacity for smelting copper concentrates without affecting normal operation, The present work eorresponds to a recent study conducted during the normal industrial operation of the Teniente Converter in this plant and, it shows the effect of increasing air oxygen enrichment from 28 to 34% on its productivity. The results show an increasing of concentrate smelting rate from 800 to 1370 tpd and hence a notorious improving in copper production, and practically no effect on the refractory consumption. The increment of the concentrate throughput, increases also the SO2 concentration and the sulfuric acid production, showing the effort done by this operation in order to accomplish the environmental Peruvian regulation,
Citation
APA:
(2003) Effect Of Oxygen Enrichment On The Teniente Converter Productivity At The Ilo Smelter, Perú (67cdbd7e-3ac1-487c-b272-f30642fb3d30)MLA: Effect Of Oxygen Enrichment On The Teniente Converter Productivity At The Ilo Smelter, Perú (67cdbd7e-3ac1-487c-b272-f30642fb3d30). The Minerals, Metals and Materials Society, 2003.