Building A Database For The Prediction Of Phases In Pt-Based Superalloys

The Southern African Institute of Mining and Metallurgy
L. A. Cornish R. Süss S. N. Prins
Organization:
The Southern African Institute of Mining and Metallurgy
Pages:
12
File Size:
1927 KB
Publication Date:
Jan 1, 2006

Abstract

The work is being done using the Thermo-CalcTM software, and the database is being built up by obtaining good thermodynamic descriptions of all of the possible phases in the system. The database supplied did not cover all of the phases, and these had to be gleaned from literature, or modelled using experimental data. Similarly, not all of the experimental data were known, and where there were gaps or inconsistencies, experiments had to be undertaken. A preliminary version of the database was constructed from assessed thermodynamic data-sets for the binary systems only. The binary descriptions were combined allowing extrapolation into the ternary systems, and experimental phase equilibrium data were compared with calculated results. Very good agreement was obtained for the Pt-Al-Ru and Pt-Cr-Ru systems, which was encouraging and confirmed that the higher-order systems could be calculated from the binary systems with confidence. Since some of the phase models in databases were different, these phases had to be remodelled. However, more work is ongoing for information concerning the ternary phases present in the Al-Cr-Ru, Pt-Al-Ru (two ternary compounds in each) and Pt-Al-Cr (possibly more than three ternary compounds) systems. At later stage of the work, problems with the thermodynamic descriptions of the Cr-Ru and Pt-Cr binary systems were found. A programme of experimental work to overcome these has been devised, and is being undertaken. Keywords: Pt-based alloys, phase diagram calculations.
Citation

APA: L. A. Cornish R. Süss S. N. Prins  (2006)  Building A Database For The Prediction Of Phases In Pt-Based Superalloys

MLA: L. A. Cornish R. Süss S. N. Prins Building A Database For The Prediction Of Phases In Pt-Based Superalloys. The Southern African Institute of Mining and Metallurgy, 2006.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account