Assessment Methodologies For Girth Weld Defects In Pipelines

Canadian Institute of Mining, Metallurgy and Petroleum
W. R. Tyson
Organization:
Canadian Institute of Mining, Metallurgy and Petroleum
Pages:
9
File Size:
469 KB
Publication Date:
Jan 1, 2010

Abstract

Imperfections such as lack-of-fusion and undercut are inevitable in field welding of pipelines. Above a certain size, such defects must be removed or repaired. In the present state of the art, determination of allowable defect size is done by Engineering Critical Assessment (ECA). This requires measurement of toughness, and comparison of toughness with crack driving force. ECA methods used in current international pipeline standards will be reviewed and compared.
Citation

APA: W. R. Tyson  (2010)  Assessment Methodologies For Girth Weld Defects In Pipelines

MLA: W. R. Tyson Assessment Methodologies For Girth Weld Defects In Pipelines. Canadian Institute of Mining, Metallurgy and Petroleum, 2010.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account