Abstract

"Studying the interaction of the phosphorus-containing flotation reagent with the components of the flotation system ""liquid-gas-solid"" during flotation of non-ferrous metal ores allows regulating the enrichment process. The phosphorus-containing reagent-collector anabasinium-O,O-dimethyl-thiophosphate has beensynthesized under laboratory conditions and the concentrated aqueous solution of anabasin hydrochloride and the 40% solution of sodium hydroxide have been used as the raw material. The phosphorus-containing reagent has been obtained by interaction of the anabasine base, sulfur and dimethyl phosphite, due to sulfur and nitrogen atoms it can form complex compounds with heavy metal ions.Studying flotation of copper-sulfide ore of the Sayak field with the use of the phosphorus-containing reagent-collector anabasinium has been performed in the open and closed cycles. The degree of ore grinding was 60- 62% of the class -0.074 mm. There has been established the dependence of the ore flotation parameters on: a) pH of the pulp; b) the consumption of the reagent-collector anabasinium.The effect of the pulp pH on the technological parameters of copper ore flotation has been carried out with a reagent regulator that increases the difference in the surface properties of the minerals to be separated.There has been used lime as the regulator of the medium, the consumption of which varied from 750 to 1500 g/t; the consumption of the reagent-collector anabasinium was 10, 15, 20 and 25 g/t.It has been found that when flotation of copper ore without the use of lime at pH equal to 7.8 and at the reagent consumption, g/t: anabasinium - 25, T-92 - 55, copper recovery in the concentrate is 92.72%, the quality of concentrate is 7, 1%.In flotation according to the factory mode (the consumption of xanthate is 44 g/t, T-92 is 55 g/t, pH = 7.8 (without lime)) of copper ore, copper recovery in the concentrate is 87.38%, the concentrate quality is 7, 97%, with reducing the xanthate consumption to 25 g/t copper recovery is reduced to 83.39%, the quality of the concentrate is up to 6.69%.In the experiments using the factory reagent mode in the closed cycle, with the xanthate mass consumption of 44 g/t, T-92 blowing agent of 55 g/t, the third recleaning concentrate contained 19.13% copper with recovery of 86.89%.Using a phosphorus-containing reagent instead of xanthate with the same flow rate, the third recleaning concentrate with the mass fraction of copper of 19.82% has beenobtained with recovery of 87.77%."
Citation

APA: N. ?. ?m?rova R. ?. Sherembayeva ?. ?. ?uktybayeva ?. B. Rakhimbekova  (2018)  Application of Phosphorus Containing Reagent at Flotation of Sulphide Copper Ore

MLA: N. ?. ?m?rova R. ?. Sherembayeva ?. ?. ?uktybayeva ?. B. Rakhimbekova Application of Phosphorus Containing Reagent at Flotation of Sulphide Copper Ore. International Mineral Processing Congress, 2018.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account