An Application of Trend Surface Analysis to the Preparation of Cover Isopach Maps for Coal Seams
- Organization:
- The Australasian Institute of Mining and Metallurgy
- Pages:
- 8
- File Size:
- 912 KB
- Publication Date:
- Jan 1, 1968
Abstract
Conventional hand drawn isopach maps of the cover of the Bulli Seam are too eomplex for use in the delineation of large domains of similar cover. Isopach maps prepared from trend surfaces fitted to the cover data are much simpler in form and so provide a convenient method of delineating broad domains of similar cover.
Citation
APA: (1968) An Application of Trend Surface Analysis to the Preparation of Cover Isopach Maps for Coal Seams
MLA: An Application of Trend Surface Analysis to the Preparation of Cover Isopach Maps for Coal Seams. The Australasian Institute of Mining and Metallurgy, 1968.