A Novel Clean Metallurgical Process for Baotou Ore:The Industrial Test Data

- Organization:
- Canadian Institute of Mining, Metallurgy and Petroleum
- Pages:
- 6
- File Size:
- 818 KB
- Publication Date:
- Jan 1, 2014
Abstract
"This paper presents the results of an industrial test using 8 t/d of Baotou concentrate (50% REO) of a clean metallurgical process, which includes: 1. Roasting with H2SO4 at low temperature (220~260 0C) in a batch roasting furnace followed by water leaching to obtain a leach liquor as feed with a yield of >95% RE and Th, recovering F as fluoride, producing a leach residue amounting to 1/3 of an equivalent high temperature residue and containing <0.03% Th and radioactivity < 3×104 Bq/kg compared to the normal high temperature residue containing 0.2-0.3% Th and 1×105 Bq/kg. 2. Separating Th with N1923 and extracting RE by P507 has been completed in mixer-settlers. Test results indicate that the ThO2 product has a purity of > 95% with a yield of 99%, and the RE has a yield of >95%, in which ThO2/REO <5×10-6, and that P507 loaded RE connect straight with separating RE using P507-HCl system. 3. Treatment and multipurpose use of "three wastes" (water, gas and solids) are discussed in some detail."
Citation
APA:
(2014) A Novel Clean Metallurgical Process for Baotou Ore:The Industrial Test DataMLA: A Novel Clean Metallurgical Process for Baotou Ore:The Industrial Test Data. Canadian Institute of Mining, Metallurgy and Petroleum, 2014.